09CuPCrNi-B plak asyese yon kalite plak asye move tan, ak 09CuPCrNi-B asye te ajoute fosfò ki fè materyèl la pi byen adapte pou aplikasyon pou gaz lafimen ak pou fasas ayestetik.

09CuPCrNi-B spesifikasyon plak asye
Steel Klas: 09CuPCrNi-B Steel Creole: GB4171-84
Epesè: 2mm-450mm, Lajè: 1000mm-4200mm, Longè: 3000mm-18000mm
|
09CuPCrNi-B Konpozisyon chimik |
|||||
|
Klas |
Eleman Max (%) |
||||
|
09CuPCrNi-B |
C |
Si |
Mn |
P |
S |
|
Mwens pase oswa egal a 0.12 |
0.10-0.40 |
0.20-0.50 |
0.06-0.12 |
Mwens pase oswa egal a 0.020 |
|
|
Kr |
Cu |
Ni |
RE |
|
|
|
0.30-0.65 |
0.25-0.45 |
0.25-0.50 |
|
|
|
Ekivalan kabòn: Ceq=【C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15】%
|
Klas |
Epesè |
Sede |
Tensile |
Elongasyon |
Eta livrezon |
|
09CuPCrNi-B |
mm |
Min Mpa |
Mpa |
% min |
|
|
4< |
295 |
431 |
24 |
Woule cho |
|
|
Mwens pase oswa egal a 4 |
265 |
402 |
27 |
Fwad woule |
09CuPCrNi-B tretman sifas plak asye: eksplozif ak penti oswa kouvwi.
09CuPCrNi-B aplikasyon plak asye
09CuPCrNi-B plak asye yo itilize pou resipyan anbake, pon asye, veso ak tank pou anpeche itilizasyon korozyon atmosferik.