Q460NH se yon asye ki gen fòs segondè, ki pi fò pase asye konvansyonèl yo, men pi ba pase klas ultra-wo fòs tankou Q500NH / Q550NH.
1. Konparezon Fòs Sede (MPa)
| Steel klas | Fòs sede (pi gran pase oswa egal a) | Nivo fòs |
|---|---|---|
| Q235NH | 235 MPa | Ba fòs |
| Q355NH | 355 MPa | Fòs mwayen |
| S355J0WP / J2WP | 355 MPa | Menm jan ak Q355NH |
| Corten A / A242 | ~345 MPa | Menm jan ak Q355NH |
| Q460NH | 460 MPa | Segondè fòs |
| Q500NH | 500 MPa | Ultra-wo fòs |
| Q550NH | 550 MPa | Ultra-wo fòs |
| Corten B / A588 | ~415–450 MPa | Yon ti kras pi ba pase Q460NH |
Q460NH se~ 105 MPa pi wopase Q355NH / S355J0WP
Q460NH se~ 40-90 MPa pi bapase Q500NH / Q550NH

2. Ranje fòs rupture
Q235NH:360–480 MPa
Q355NH / S355J0WP:470–630 MPa
Q460NH:550–710 MPa
Q500NH / Q550NH:600–780 MPa
3. Avantaj konsepsyon estriktirèl
Anba menm chaj la:
Q460NH ka itilizepi mens plak / pi piti seksyonpase Q355NH
Diminye pwa estriktirèl, amelyore kapasite span, diminye pri fondasyon
4. Severite ak soudabilite komès-off
Pi wo fòs tou pote dezavantaj ti tay:
Kabòn ekivalan pi wo →yon ti kras pi mal soudabilite
Ka mande pou prechofaj pou plak epè
Severite tanperati ki ba yon ti kras pi ba pase Q355NH