ASTM A709se spesifikasyon estanda pou asye estriktirèl yo itilize nan konstriksyon pon, eleman chaj-pote, ak estrikti sipò kritik.

info-601-601

Espesifikasyon sa a kouvri asye kabòn, gwo -fòs ba-alyaj estriktirèl plak asye ak ba, osi byen ke plak alyaj trempe ak tanperaman ki fèt pou fòs ak pèfòmans siperyè.

 

ASTM A709 gen ladan plizyè klas ak diferan nivo fòs rupture pou satisfè kondisyon jeni divès kalite.

 

Gnee Disponib Size Range

 

Epesè: 12 mm - 50 mm

Lajè: 400 mm - 1200 mm

Longè: 600 mm - 2800 mm

Materyèl ekivalan: GB Q345Q

 

ASTM A709 Klas 50 Konpozisyon Chimik

 

Materyèl C Si Mn P S Nb + V (max)
A709 Gr 50 Mwens pase oswa egal a 0.23 Mwens pase oswa egal a 0.40 Mwens pase oswa egal a 1.35 Mwens pase oswa egal a 0.04 Mwens pase oswa egal a 0.05 0.02–0.15

 

ASTM A709 Klas 50 Pwopriyete mekanik

 

 

Materyèl Fòs Sede (MPa) Fòs rupture (MPa) Elongasyon δ200 (%)
A709 Gr 50 345–470 450–600 21–35

 

Poukisa chwazi Gnee pou plak asye A709 klas 50?

 

Gnee apwovizyone plak asye ki wo-woule prim epi li gen anpil eksperyans nan ekspòte asye estriktirèl-atravè lemond. Stock nou an gen ladan yon seleksyon lajè ASTM A709 plak, asire livrezon rapid ak bon jan kalite serye pou pon ak pwojè enfrastrikti.

 

Senpleman pataje dimansyon ak kantite ou bezwen yo - Gnee pral ede w jwenn bon materyèl A709 Klas 50 la ak pri konpetitif ak sipò pwofesyonèl.

 

Kontakte nou jodi a pou yon sitasyon sou ASTM A709 Gr 50 plak asye.

 

Kontakte kounye a

 

info-627-561

Ki sa ki A709 klas 50W asye?

ASTM A709-50W seyon spesifikasyon estanda pou asye estriktirèl prensipalman nan fabwikasyon an nan pon asye. ASTM A709-50W kouvri gwo fòs, ba pèmèt fòm estriktirèl asye, plak ak ba.

 

Ki klas ASTM A709 asye?

ASTM A709 la se spesifikasyon estanda pou asye estriktirèl pou pon epi li gen ladan kabòn, segondè -fòs ki ba- alyaj, ak asye alyaj trempe ak tanperaman yo itilize kòm plak estriktirèl nan konstriksyon an nan pon yo. SSAB ofri senk klas sa yo nan A709;36, 50, 50W, HPS 50W ak HPS 70W.

 

Ki diferans ki genyen ant ASTM A572 Klas 50 ak ASTM A709 Klas 50?

A572 Klas 50: Itilize nan yon pakèt aplikasyon estriktirèl, tankou bilding, gwo fò tou won transmisyon, ekipman, ak konstriksyon jeneral. Li pa espesyalman optimize pou pon yo. A709 Klas 50: Prensipalman yo itilize pou konstriksyon pon ak lòt estrikti kote rezistans amelyore ak soudabilite yo enpòtan.

 

Ki fòs sede ASTM A709 klas 50?

Klas 50 asye nan spesifikasyon sa a mande pou yon fòs sede minimòm de 50 ksi. Itilize kòm manm estriktirèl nan bilding pon oswa pou estrikti menm jan an.

 

Ki diferans ki genyen ant ASTM A36 ak A709?

ASTM A709 klas 36 se yon materyèl pon kote kabòn ajoute nan fòs ak hardenability nan asye a.A36 gen mwens pase0. 30% kabòn e konsa, pa posede gwo hardenability. Plak asye ASTM A709 klas 36 amelyore rezistans korozyon epi yo ka itilize nan aplikasyon deyò.

 

Ki sa ki ekivalan ASTM A572 klas 50?

ASTM A572 Klas 50 ekivalan a plizyè lòt klas asye, ak ekivalan entènasyonal ki pi komen yo se S355JR (estanda Ewopeyen an) ak Q345B (estanda Chinwa). Pi bon ekivalan a depann sou kondisyon espesifik pwojè yo, kidonk li toujou pi bon pou konsilte espesifikasyon materyèl ak yon espesyalis pou konfime konpatibilite.

 

Ki diferans ki genyen ant ASTM A36 ak ASTM A572 GR 50?

Kòm mansyone pi bonè,A36 se asye ki gen yon fòs sede minimòm de 36,000 PSI. Klas sa a soti fòs li nan yon konbinezon kabòn ak Manganèz. Nan lòt men an, A572-50, pou egzanp, se yon kalite asye ak yon fòs sede minimòm de 50,000 PSI.

 

Ki diferans ki genyen ant A572 ak s355?

An rezime, tou de ASTM A572 Klas 50 ak S355JR yo se chwa ekselan pou aplikasyon asye estriktirèl, akASTM A572 Klas 50 bay pi gwo kapasite fòs ak S355JR ofri adaptabilite ak itilizasyon toupatou nan pwojè konstriksyon Ewopeyen an..

 

Èske A572 asye korozyon reziste?

A572 asye se tipikman itilize nan aplikasyon estriktirèl akòz gwo fòs li yo, duktilite, soudabilite akrezistans korozyon. Aplikasyon sa yo gen ladan seksyon estriktirèl, ba ranfòsman, pon, gratsyèl ak kay.

 

Klas Kabòn ak Ba-alyaj segondè-Fòs Asye ki founi pa GNEE
ASTM/ASME ASTM A36/A36M ASTM A36      
ASTM A283/A283M ASTM A283 Klas A ASTM A283 Klas B ASTM A283 Klas C ASTM A283 Klas D
ASTM A514/A514M ASTM A514 Klas A ASTM A514 Klas B ASTM A514 Klas C ASTM A514 Klas E
ASTM A514 Klas F ASTM A514 Klas H ASTM A514 klas J ASTM A514 Klas K
ASTM A514 Klas M ASTM A514 Klas P ASTM A514 Klas Q ASTM A514 Klas R
ASTM A514 Klas S ASTM A514 Klas T    
ASTM A572/A572M ASTM A572 Klas 42 ASTM A572 Klas 50 ASTM A572 Klas 55 ASTM A572 Klas 60
ASTM A572 Klas 65      
ASTM A573/A573M ASTM A573 Klas 58 ASTM A573 Klas 65 ASTM A573 Klas 70  
ASTM A588/A588M ASTM A588 Klas A ASTM A588 Klas B ASTM A588 Klas C ASTM A588 Klas K
ASTM A633/A633M ASTM A633 Klas A ASTM A633 Klas C ASTM A633 Klas D ASTM A633 Klas E
ASTM A656/A656M ASTM A656 Klas 50 ASTM A656 Klas 60 ASTM A656 Klas 70 ASTM A656 Klas 80
ASTM A709/A709M ASTM A709 Klas 36 ASTM A709 Klas 50 ASTM A709 Klas 50S ASTM A709 Klas 50W
ASTM A709 klas HPS 50W ASTM A709 klas HPS 70W ASTM A709 Klas 100 ASTM A709 Klas 100W
ASTM A709 klas HPS 100W      
ASME SA36/SA36M ASME SA36      
ASME SA283/SA283M ASME SA283 Klas A ASME SA283 Klas B ASME SA283 Klas C ASME SA283 Klas D
ASME SA514/SA514M ASME SA514 Klas A ASME SA514 Klas B ASME SA514 Klas C ASME SA514 Klas E
ASME SA514 Klas F ASME SA514 Klas H ASME SA514 Klas J ASME SA514 Klas K
ASME SA514 Klas M ASME SA514 Klas P ASME SA514 Klas Q ASME SA514 Klas R
ASME SA514 Klas S ASME SA514 Klas T    
ASME SA572/SA572M ASME SA572 Klas 42 ASME SA572 Klas 50 ASME SA572 Klas 55 ASME SA572 Klas 60
ASME SA572 Klas 65      
ASME SA573/SA573M ASME SA573 Klas 58 ASME SA573 Klas 65 ASME SA573 Klas 70  
ASME SA588/SA588M ASME SA588 Klas A ASME SA588 Klas B ASME SA588 Klas C ASME SA588 Klas K
ASME SA633/SA633M ASME SA633 Klas A ASME SA633 Klas C ASME SA633 Klas D ASME SA633 Klas E
ASME SA656/SA656M ASME SA656 Klas 50 ASME SA656 Klas 60 ASME SA656 Klas 70 ASME SA656 Klas 80
ASME SA709/SA709M ASME SA709 Klas 36 ASME SA709 Klas 50 ASME SA709 Klas 50S ASME SA709 Klas 50W
ASME SA709 klas HPS 50W ASME SA709 klas HPS 70W ASME SA709 Klas 100 ASME SA709 Klas 100W
ASME SA709 klas HPS 100W      
EN10025 EN10025-2 EN10025-2 S235J0 EN10025-2 S275J0 EN10025-2 S355J0 EN10025-2 S355K2
EN10025-2 S235JR EN10025-2 S275JR EN10025-2 S355JR EN10025-2 S420J0
EN10025-2 S235J2 EN10025-2 S275J2 EN10025-2 S355J2  
EN10025-3 EN10025-3 S275N EN10025-3 S355N EN10025-3 S420N EN10025-3 S460N
EN10025-3 S275NL EN10025-3 S355NL EN10025-3 S420NL EN10025-3 S460NL
EN10025-4 EN10025-4 S275M EN10025-4 S355M EN10025-4 S420M EN10025-4 S460M
EN10025-4 S275ML EN10025-4 S355ML EN10025-4 S420ML EN10025-4 S460ML
EN10025-6 EN10025-6 S460Q EN10025-6 S460QL EN10025-6 S460QL1 EN10025-6 S500Q
EN10025-6 S500QL EN10025-6 S500QL1 EN10025-6 S550Q EN10025-6 S550QL
EN10025-6 S550QL1 EN10025-6 S620Q EN10025-6 S620QL EN10025-6 S620QL1
EN10025-6 S690Q EN10025-6 S690QL EN10025-6 S690Q1 EN10025-6 S890Q
EN10025-6 S890QL EN10025-6 S890QL1 EN10025-6 S960Q EN10025-6 S960QL
JIS JIS G3101 JIS G3101 SS330 JIS G3101 SS400 JIS G3101 SS490 JIS G3101 SS540
JIS G3106 JIS G3106 SM400A JIS G3106 SM400B JIS G3106 SM400C JIS G3106 SM490A
JIS G3106 SM490YA JIS G3106 SM490B JIS G3106 SM490YB JIS G3106 SM490C
JIS G3106 SM520B JIS G3106 SM520C JIS G3106 SM570  
DIN DIN 17100 DIN17100 St52-3 DIN17100 St37-2 DIN17100 St37-3 DIN17100 RSt37-2
DIN17100 USt37-2      
DIN 17102 DIN17102 StE315 DIN17102 EStE315 DIN17102 TStE315 DIN17102 WStE315
DIN17102 StE355 DIN17102 EStE355 DIN17102 TStE355 DIN17102 WStE355
DIN17102 StE380 DIN17102 EStE380 DIN17102 TStE380 DIN17102 WStE380
DIN17102 StE420 DIN17102 EStE420 DIN17102 TStE420 DIN17102 WStE420
DIN17102 StE460 DIN17102 EStE460 DIN17102 TStE460 DIN17102 WStE460
DIN17102 StE500 DIN17102 EStE500 DIN17102 TStE500 DIN17102 WStE500
DIN17102 EStE285      
GB GB/T700 GB/T700 Q235A GB/T700 Q235B GB/T700 Q235C GB/T700 Q235D
GB/T700 Q275      
GB/T1591 GB/T1591 Q345A GB/T1591 Q390A GB/T1591 Q420A GB/T1591 Q420E
GB/T1591 Q345B GB/T1591 Q390B GB/T1591 Q420B GB/T1591 Q460C
GB/T1591 Q345C GB/T1591 Q390C GB/T1591 Q420C GB/T1591 Q460D
GB/T1591 Q345D GB/T1591 Q390D GB/T1591 Q420D GB/T1591 Q460E
GB/T1591 Q345E GB/T1591 Q390E    
GB/T16270 GB/T16270 Q550C GB/T16270 Q550D GB/T16270 Q550E GB/T16270 Q550F
GB/T16270 Q620C GB/T16270 Q620D GB/T16270 Q620E GB/T16270 Q620F
GB/T16270 Q690C GB/T16270 Q690D GB/T16270 Q690E GB/T16270 Q690F
GB/T16270 Q800C GB/T16270 Q800D GB/T16270 Q800E GB/T16270 Q800F
GB/T16270 Q890C GB/T16270 Q890D GB/T16270 Q890E GB/T16270 Q890F
GB/T16270 Q960C GB/T16270 Q960D GB/T16270 Q960E GB/T16270 Q960F
GB/T16270 Q500