Ki diferans ki genyen ant SPA-woule frèt ak cho-woule SPA-H an tèm de pwopriyete mekanik?

Jan 21, 2026 Kite yon mesaj

Diferans pwopriyete mekanik ant frèt-woule ak cho-woule SPA-H Weathering Steel plak

 
Diferans debaz la soti nanwoule frèt-pwovoke travay di(deformation plastik -tanperati chanm) nan frèt-woule SPA-H, ki amelyore fòs/dite men diminye duktilite, pandan y ap cho-woule SPA-H kenbe yon mikwostrikti balanse, san rèd ak pi bon fòmabilite-tou de satisfè kondisyon mekanik JIS G 317{5} ak limite debaz mekanik{17} 1.6-6 mm kalib ak cho -woule ki kouvri tout epesè komèsyal (1.6-100 mm).

info-609-368

Sede fòs: Fwad-woule=415–450 MPa (20–30% pi wo pase cho-woule); Cho -woule=345–420 MPa (JIS min 345 MPa).

 

Fòs rupture: Fwad-woule=550–600 MPa (15-25% pi wo pase cho-woule); Cho -woule=480–620 MPa (JIS min 480 MPa).

 

Brinell dite: Fwad-woule=210–270 HBW (15-25% pi wo pase cho-woule); Cho -woule=180–220 HBW.

 

Allongement nan Break: Fwad-woule=≤15% (gout enpòtan, fòmabilite pòv); Cho -woule=≥20% (bon duktilite pou fòme).

 

Severite: Fwad-woule te yon ti kras redwi ba-tanperati rezistans; Cho -woule kenbe ki estab anbyen/ba-tanperati enpak rezistans (40-50 J chanm-tanperati Charpy V-dan).

 

Estrès rezidyèl: Fwad-woule gen gwo estrès rezidyèl entèn (ki soti nan travay di); Cho -woule gen estrès rezidyèl ki ba, ki gaye (pa gen okenn redi travay grav).